Title: Solutions in Automated Blast Cleaning
Author: Herb Tobben, Manager
Source: ABC, Vol 4/ No 2, Spring 1999
Publication year 1999
Document number: 1999116
Number of pages: 2
Abstract:
"Thank you" to Clemco Industries for allowing us to share with you infomation from their newsletter ZERO Update. The following covers the work of Herb Tobben, the manager
of ZERO's Sample Processing Lab. Jack Champaigne of Electronics Incorporated recently toured Clemco/ZERO and he especially enjoyed his visit with Herb at the Sample
Processing facility. Herb has been a guest speaker at the EI annual shot peening workshops since 1996- we think that his work is very valuable and interesting.
Reprinted with permission
CREATING QUIETER, MORE DURABLE GEARS:
A major U.S. manufacturer of automotive gears asked ZERO for help with two problems common in multi-step machinging operations. The company makes a variety of gears for use
in transmissions, transfer cases (for four-wheel drive vehicles), and differentials.