Title: Process for Increasing the Lifespan of Dental Components
Author: G Lange; F-J Grau, both of Germany
Source: US Patent 6,012,316
Publication year 2000
Document number: 2000014
Number of pages: 7

Abstract:
With a view to increasing the lifespan of metallic dental components as regards fatigue fractures, compressive stresses are introduced into the surface layer of these components, such as by means of shot-peening.