ZERO Products Div., Clemco Industries Corp.
2001 Clemco Industries Corp.
Reprinted with permission
The Problem:
A glass manufacturer was experiencing a lot of stress while cutting glass slabs. These "glass ingots" measure up to three feet by two feet, three inches thick, and weight up
to 150 pounds. The customer uses a diamond saw to cut the slab into strips, with the cut pieces going on to further processing, including meticulousness grinding and
polishing. They eventually become precision laser lenses.