Title: Shot Peening In Maintenance Of Steel Structures
Author: Salko Djozic
Source: Conf Proc: ICSP & BC - 2
Publication year 2001
Document number: 2001181
Number of pages: 3
Abstract:
Guidelines for choosing appropriate intensity for the desired
results of Shot Peening originated from car design and shot
peening was found to impart 40% greater efficiency to car
structures (SAE 1973). Saving on the weights of valves, gears,
shafts, chambers, pressure vessels and steel weights made car
design more competitive.