Title: Shot Peening of Cast Magnesium Alloys
Author: Ludian, Hilpert, Kiefer, Wagner
Source: Conf Proc: ICSP-8 Sept. 16-20, 2002 Garmisch-Partenkirchen, Germany (pps. 3
Publication year 2002
Document number: 2002048
Number of pages: 6
Abstract:
Authors
Tomasz Ludian 1), Matthias Hilpert 2), Armin Kiefer 3) and Lothar Wagner 1)
1) Chair of Physical Metallurgy and Materials Technology, Technical University of Brandenburg at Cottbus, Cottbus, Germany
2) Otto Fuchs Metallwerke, Meinerzhagen, Germany
3) OSK Kiefer, Oppurg, Germany
Abstract
The fatigue behavior of the high-pressure die cast magnesium alloys AM50 and AZ91 was investigated. In both alloys, cast defects led to marked scatter in fatigue
performance.
To study potential improvements in fatigue behavior, shot peening was performed using various Almen intensities. Both alloys showed marked improvements in fatigue strength
compared to an electropolished reference.