Title: Effect of Test Temperature on Fatigue of Shot Peened Magnesium Alloys
Author: Wendt, Ketzmer and Wagner
Source: Conf Proc: ICSP-8 Sept. 16-20, 2002 Garmisch-Partenkirchen, Germany
Publication year 2002
Document number: 2002050
Number of pages: 6
Abstract:
Authors
Jens Wendt, Andre Ketzmer and Lothar Wagner
Chair of Physical Metallurgy and Materials Technology, Technical University of Brandenburg at Cottbus, Cottbus, Germany
Abstract
The effect of test temperature ranging from -25 to +50 C on mechanical properties of the high-strength wrought magnesium alloy AZ80 was evaluated. While yield stress and
tensile strength within this temperature range continuously increased with decreasing temperature, the 10 7 cycles notch fatigue strength in fully reversed loading exhibited
a marked minimum at T = 0 C. Shot peening was found to improve the fatigue strength at all tested temperatures.