Abstract:
Authors
Chris A. Rodopoulos 1, Rachel E. Edwards 1, Sean Curtis 1, Jose Solis Romero 1, Jung-Hee Choi 1,2, Eduardo de los Rios 1 and Andrew Levers 3
1 Division of Aeronautical Applications, Department of Mechanical Engineering, University of Sheffield, Sheffield, UK
2 Hyundai Motor Company, S. Korea
3 Airbus UK, Chester, UK
1 Introduction
For many years controlled shot peening (CSP) was considered as a surface treatment of questionable benefits. This impression was fuelled by contradictory results from
fatigue experiments [1,2]. It is now clear that the performance of CSP in terms of fatigue depends on the balance between its beneficial (compressive residual stress and
work hardening) and detrimental effects (surface roughening) [3,4]. Hence, in order to achieve a favourable fatigue performance, the role of those effects has to be analysed
and understood. To achieve such undertaking it is essential to consider their interaction with other parameters such as the nature of the target material and the loading
conditions.
This work brings together two micromechanical models, (i) for notch sensitivity [5] and (ii) for fatigue life [6]. The former assesses the effect of surface roughening,
whilst the latter incorporates the residual stress distribution and work hardening on fatigue life calculations. Combination of the two models allows the determination of
the residual stress distribution to meet specific improvements in fatigue life (improvement life factor, ILF). Using the ILF methodology, the effects of CSP can be
scrutinised against stress level, surface roughness and ILF value.