Title: Finite Element Simulation of Shot Peen Forming
Author: Zang
Source: Conf Proc: ICSP-8 Sept. 16-20, 2002 Garmisch-Partenkirchen, Germany
Publication year 2002
Document number: 2002072
Number of pages: 8
Abstract:
Author
Yuansong Zeng
Beijing Aeronautical Manufacturing Technology Research Institute, Beijing, P.R. China
1 Abstract
In this paper, both the impact model and the forming process simulation of the shot peen forming are introduced. In the impact model, effects of the shot diameter and
velocity on the value and depth of the compressive stress and plastic layer are analyzed with dynamic explicit finite element method (FEM). A new equivalent thermal loading
method is presented for the simulation of the shot peen forming process. The deformation of the standard Almen Strip and a wing skin with ribs are simulated with the method
using static implicit FEM software. Results show that the method is very effective if the relationships between thermal loads and the shot peening strength are suitably set
up.
Download full text pdf file