Title: The Strength of the Smoothness
Author: Franck Petit-Renaud, M. Phil., B.Sc., DUT
Source: TSP, Vol 16 / Issue 2, Summer 2002
Publication year 2002
Document number: 2002096
Number of pages: 2

Abstract:
A case study by Franck Petit-Renaud, M. Phil., B.Sc., DUT. USF Impact Finishers (Shot Peening Division), June 2001 Introduction: This short article will aim to present two techniques used to enhance fatigue strength and fatigue life of components such as gears as well as other transmission components.