Title: Shot Peening of Metal Parts
Author: General Electric
Source: GE P11TF3 S-17
Publication year 2003
Document number: 2003002
Number of pages: 41
Abstract:
1. SCOPE
1.1 Scope. This specification presents requirements for shot peening of metal parts to induce residual compressive stresses in specified surfaces, for the purpose of
preserving the fatigue strength and increasing resistance to stress corrosion cracking and fretting.
This article not available