Electronics Incorporated - The Shot Peener - Shot Peening Library

Title: Test Strip Holder for Supporting Test Strips Measuring the Intensity of Shot Peening in Cavities
Author: Erwin Baiker, Glattbrugg (CH)
Source: US Patent 6,502,449 B1
Publication year 2003
Document number: 2003004
Number of pages: 9
Abstract:
A holder for mounting a test strip for measuring the intensity of shot peening in internal cavities includes a receptacle receiving any of multiple inserts configured to
form a segment of an internal cavity of a component to be peened. The test strip defines the remainder of the cavity. The shot stream to be measured is introduce into the
cavity, after which the test strip is removed and measured in the conventional manner. Accordingly, the intensity of peening in internal cavities may be measured with
relative accuracy. By providing multiple inserts, intensity of peening in cavities of varying sizes may be measured by simply changing the insert.
Download full text pdf file
www.shotpeener.com
This page last revised: 04/24/2008