Abstract:
ABSTRACT
Material for a connecting rod for an internal combustion engine is carburized and quenched, a carburized layer formed on the bearing portion is ground until the portion
which exhibits the maximum compressive residual stress, and a shot-peening processing is performed on the ground surface. The invention produces a bearing portion having
surface characteristics in which maximum compressive residual stress is imparted, and therefore, remarkable improvement in the fatigue strength in the bearing portion can be
obtained. Furthermore, a large number of concavities formed by the shot-peening processing can be efficiently employed as an oil reservoir, so that sliding properties and
lubrication can be improved, and the occurrence of problems such as fretting corrosion, galling, and seize can also be solved, and the galling and problems of the seize can
be prevented.