Title: Optimization of Residual Stress and Fatigue Life in Laser Peened Componts
Author: MR Hill, TE Pistochini, AT DeWald
Source: Conf Proc: ICSP-9 (pg 156-162)
Publication year 2005
Document number: 2005066
Number of pages: 7

Abstract:
ABSTRACT Laser peening is an emerging technology for the surface treatment of metallic materials that is capable of enhancing resistance to fatigue failure. This paper describes some recent results from joint research programs conducted to generate data on residual stress and fatigue performance of laser peened materials. Specifically, we present data for residual stress imparted by laser peening and fatigue life improvement of laser peened coupons relative to as-machined coupons. These data are presented for a range of high-strength materials employed in aircraft and other demanding applications: BSTOA Ti6AI-4V titanium alloy, 300M steel, MP35N Ni-Co-Cr-Mo alloy, and 7050-T7451 aluminum alloy. For each material, residual stress distributions were measured for treatment with different laser peening parameter sets. For particular laser peening parameter sets, stress versus life data were generated for as-machined and laser peened fatigue coupons, which quantifies fatigue life improvement attained by laser peening over a range of applied loads.


Click here to download full text pdf file

www.shotpeener.com
This page last revised: 10/22/2009
spc2003a.frx