Abstract:
ABSTRACT Kugelstrahlzentrum Aachen GmbH (KSA), a company specialized in shot peening services and automation solutions, and Rolls-Royce Deutschland (RRD), a subsidiary of Rolls-Royce plc, are currently working together to develop and test an improved process control system for shot peening applications. The common goal is a system for monitoring peening intensities on-line in order to reduce Almen tests and consequently to cut process times and costs. In the context of this joint project, KSA has down-scaled its shot velocity measurement system to measure smaller shot sizes down to 0.1 mm. The ISIC-system (Integral Shot Intensity Control) is able to detect shot velocities of ferrous and non-ferrous peening media as well as mixtures of different media sizes. The main results are at present: A clear linear correlation with Almen intensities, even higher sensitivity and an ability to quantify the influence of varying shot sizes and particle distribution.


Click here to download full text pdf file

www.shotpeener.com
This page last revised: 10/22/2009
spc2003a.frx