Abstract:
This Standard establishes the procedures for controlled shot peening or glass bead peeing of steel, titanium, aluminum or magnesium parts, to induce residual compressive stresses in specified surfaces, for the purpose of increasing the fatigue strength and resistance to stress corrosion cracking.