Electronics Incorporated - The Shot Peener - Shot Peening Library


Title: Covering the Basics: Intensity & Coverage
Author: Jack Champaigne
Source: TSP, Vol 21/ Issue 1, Winter 2007
Publication year 2007
Document number: 2007002
Number of pages: 2

Abstract:
During an on-site training program, the Electronics Inc. training staff is available to answer questions and address problems. While some problems are unique to each facility, we find that both new and experienced personnel in shot peening are often challenged by the concept of appropriate peening coverage, and the confusion is often related to the saturation curve.


Download full text pdf file

www.shotpeener.com
This page last revised: 03/04/2009