Abstract:
A flat piece of leaf spring has, since the days of the blacksmith, received continued impacts of the hammer long after cooling down in temperature. Though the blacksmith didn't always realize the effects of his actions, it is now known that the life of this leaf spring is enhanced by upwards of 600% by such an action!