Title: The Marketing of Barkhausen Noise Analysis
Author: Michel Cardon
Source: TSP Volume 21 / Issue 2, Spring 2007
Publication year 2007
Document number: 2007011
Number of pages: 2
Abstract:
Twenty years ago, I read about a group of Finnish scientists who concentrated on an obscure phenomenon-Barkhausen Noise.
This phenomenon was unknown at that time, at least by those who could usefully apply it to their quality control problems. I was one of them, researching how shot peened
parts could be controlled in production.
Download full text pdf file