A successful titanium metal powder process would provide components with the same strength and weight advantages has products made from large, solid pieces of titanium, at a
fraction of their present cost. Currently, few industries can justify titanium's high price tag. The opportunities are tremendous for companies that can bring a viable
titanium metal powder process to market.