Title: Properties of Air-Blast Shot Streams
Author: David Kirk
Source: TSP, Vol 22 / Issue 1, Winter 2008
Publication year 2008
Document number: 2008004
Number of pages: 5
Abstract:
INTRODUCTION
Shot peening involves three factors - Shot Stream, Machine and Workpiece. These three factors interact to determine the prime-objective parameters of coverage and peening
intensity. Fig. 1 illustrates these interactions.