Title: Bringing Specs into the 21st Century
Author: Jack Champaigne, Electronics Inc
Source: TSP, Vol 22 / Issue 2, Spring 2008
Publication year 2008
Document number: 2008011
Number of pages: 1

Abstract:
Editorial Jack Champaigne Shot Peening specs written in the 1940s by OEMs just don't make sense for today's MROs, job shops, product and media manufacturers. As a member of AMEC (Aerospace Metals Engineering Committee of the Aerospace Materials Division of the Society of Automotive Engineers), I have the opportunity to contribute to the evolution of shot peening specifications.