Title: An Unlikely Partnership Uncovers Superior Masking Products
Author: The Shot Peener Staff
Source: TSP, Vol 22 / Issue 3, Summer 2008
Publication year 2008
Document number: 2008026
Number of pages: 1

Abstract:
When Goodrich Engine Components was looking for a shot peening masking resource, they found an unlikely partner with Maxol Studios. Maxol Studios is known for its industry-leading silicone tooling and resin casting technologies but these processes had been focused on the Rapid Prototyping / Rapid Manufacturing industry. Working closely with Goodrich engineers, Maxol Studios applied their unique and effective tooling and molding talents to create durable shot peen masking from high performance polyurethane casting resins.