Title: Aerospace Shot Peening Practices And Nadcap
Author: Champaigne, Jack
Source: Conf Proc: ICSP-10 Tokyo, Japan 2008
Publication year 2008
Document number: 2008029
Number of pages: 4
Abstract:
Shot peening practices are highly controlled by both proprietary and industry standard specifications. There are many cases where Industry standards, such as SAE J442 and
J443 or AMS 2430, are incorporated into proprietary practices. Audits to confirm compliance to an industry concensus standard are offered by Preformance Review Insistute
(PRI) in the form of Nandcap Audits.
KEY WORDS
Shot Peening audits, Nadcap shot peening audits,