Electronics Incorporated - The Shot Peener - Shot Peening Library

Title: A Case of Shot Peening Fraud
Author: The Shot Peener Staff
Source: TSP, Vol 22 / Issue 4, Fall 2008
Publication year 2008
Document number: 2008035
Number of pages: 4
Abstract:
Feature Story A Case of Shot Peening Fraud
File Name: 06a0766n.06
Filed: October 17, 2006
Case No. 05-3267
United States Court of Appeals for the Sixth Circuit
United States of America, Plaintiff-Appellee, v.
Se Keun Oh, a.k.a. JIMMY OH, Defendant-Appellant
On appeal from the United States District Court for
the Northern District of Ohio
Before: Batchelder, Griffen, Circuit Judges; and
Zatkoff, District Judge.
ALICE M. BATCHELDER, Circuit Judge. Defendant-Appellant Se Keun “Jimmy” Oh (“Mr. Oh”) was indicted on charges of wire fraud in violation of 18 U.S.C. § 1343 (Counts 1, 2 and
3) and making false statements with regard to several government contracts for military parts, in violation of 18 U.S.C. § 1001(a) (Counts 4, 5, 6 and 7). The jury acquitted
him on Count 4 and convicted him on all other counts, and Mr. Oh appeals, claiming that the evidence was insufficient to support his conviction on Count 1and that the
district court erred in permitting the jury to consider certain evidence to which Mr. Oh timely objected. Finding no error in either regard, we affirm the conviction.
Click here to download full text pdf file