Abstract:
ABSTRACT Shot peening improves contact fatigue strength of mechanical components due to work hardening. However, in the case of components used under high pressure such as gears of automotive transmission, temperature of the contact part elevated over 200 due to frictional heat. Therefore, it was expected that the part cause reduction of beneficial effect of shot peening via temper softening. In this research, softening behavior of shot peened carburized steel due to elevated temperature was investigated, and then the effect of shot peening in high temperature was considered. KEY WORDS Carburized steel, Temper, Softening, Vickers hardness, Auto motive gear

This ICSP paper is not available until September of 2011. You may purchase the complete conference procedings ICSP-10 for $230 at Electronics Inc +1-574-256-5001

www.shotpeener.com
This page last revised: 03/22/2010
spc2003a.frx