Abstract:
ABSTRACT
In order to satisfy stringent requirements regarding reliability, minimum weight, high performance, cost-effectiveness and long-term durability, the components of modern
aircraft engines must tap the full potential of the materials used. For this reason, there has been a growing interest in work hardening processes applied to the surface
layers of highly-stressed components with particular attention drawn towards the optimisation of established techniques such as shot peening and deep rolling as well as the
development of new methods. Such a new method is the ultrasonic impact treatment (UIT). UIT is predominantly used in the manual post-weld processing of steels. In addition
to the intrinsic local
and low loading treatment, UIT is cost-effective and easy to control such that it may be suitable for a wide range of applications. The objective of this work is to describe
the potential of applying UIT to the high-strength nickel base alloy IN718. In order to characterise the hardened surface layer, surface roughness measurements and Xray
residual stress analyses were taken including experiments to evaluate the thermal stability of selected samples. The results obtained were compared to shot peened and deep
rolled surfaces. It was discovered that the UIT technique produces deep surface layer work hardening. The hardening depths and surface roughnesses are similar to that
obtained by deep rolling. Therefore all the specific advantages of UIT can be extended to the surface hardening of aero engine components.
KEYWORDS
Ultrasonic impact treatment, surface treatment, work hardening, residual stresses, IN718