Title: Effect Of Deep Rolling On The Cyclic Performance Of Magnesium And Aluminum Alloys In The Temperature Range 20-250°c
Author: Altenberger, Wagner, Mhaede, Juijerm, Noster
Source: Conf Proc: ICSP-10 Tokyo, Japan 2008
Publication year 2008
Document number: 2008127
Number of pages: 6

Abstract:
ABSTRACT Mechanical surface treatments such as deep rolling or laser-shock peening can markedly affect the cyclic performance of light-weight alloys, especially if significantly thick work hardened surface regions are induced. At room temperature, the cyclic deformation behaviour is strongly influenced by the nature of the induced near-surface microstructures provided that they remain stable during fatigue loading. At elevated temperatures, the stability of near-surface work hardening and local microstructures plays an even more important role since the process-induced residual compressive stresses are likely to anneal out partially or completely. This overview illustrates to what extent deep rolling can affect the cyclic performance of various light alloys being fatigue loaded in stress control at ambient and elevated temperatures. KEY WORDS Deep Rolling, Aluminum Alloys, Magnesium Alloys, High Temperature Fatigue

This ICSP paper is not available until September of 2011. You may purchase the complete conference procedings ICSP-10 for $230 at Electronics Inc +1-574-256-5001

www.shotpeener.com
This page last revised: 03/22/2010
spc2003a.frx