Abstract:
Featured Article Flapping Peening Picks Up Speed
Flapper peening (also called roto-peening) looks like such a small, delicate process—more like jewelry making than shot peening. But don’t let the equipment size fool you.
Flapper peening’s benefits are huge and its usage is growing in aerospace maintenance, repair and overhaul (MRO) facilities.