Electronics Incorporated - The Shot Peener - Shot Peening Library

Title: Intensity Investigation
Author: Shot Peener Staff
Source: TSP, Vol 23 / Issue 2, Spring 2009
Publication year 2009
Document number: 2009010
Number of pages: 2
Abstract:
The Electronics Inc. staff is often called upon
The Electronics Inc. staff is often called upon to solve shot peening mysteries. The usual villain is a lack of intensity control. Intensity control problems have many
sources and the most common are:
1. A lack of understanding of the intensity measurement process
2. Poor media management
3. Equipment maintenance issues
The following field report from an in-house shot peening shop visit has a sampling of problems in each area.