Abstract:
Switching Over: Peening with a Cleaning Machine Present times call for innovative approaches. If your blast cleaning workload has decreased, can you take on peening projects to put idle machinery to work? Yes, there might be business out there that won’t require a big investment to get it; however, it is important to understand the differences between blast cleaning and shot peening before you make any changes.