Title: SAE Specifications Update
Author: Jack Champaigne
Source: TSP, Vol 23 / Issue 3, Summer 2009
Publication year 2009
Document number: 2009030
Number of pages: 1

Abstract:
The Parting Shot As chairman of the Surface Enhancement Division of the Fatigue Design and Evaluation Committee, I have had a unique opportunity to participate in the development of shot peening standard practices. I have witnessed the evolution of concerns from media production and maintenance issues to practices of determination of coverage and measurement of intensity. Throughout this association I am impressed with the enthusiasm of the many dedicated committee members that forge ahead with new and exciting practices.