Hi All,

Our customer drawing required shot peening with below shot:
SHOT SIZE 550
INTENSITY 12-14C
COVERAGE 200%
SHOT TYPE NON MAG

Non Mag shot is very new to me. Please help me explain "non mag shot" is made from what material?

Thank you and appreciate your support.
Liked Replies
#1553 Oct 14th a 01:39 PM
by Very Old Tom
Very Old Tom
Hi, Donhan,
You may well have solved this problem but just for the record, you could try using Guysons Spherically Conditioned Stainless Steel Cut Wire Shot. it comes in many sizes, the closest to 550 would probably be made from the Ø1.5mm cut wire.