Catch test on glass bead - 08/14/06 10:31 AM
Hi,
I'm trying to perform catch tests for flow valve calibration on an equipment that uses MIL-11 (AGB-10) glass bead. This grade being very fine, I'm having problems finding a way to keep the media in the catch test container without causing restriction for the air to get out. Anyone has experience in using this media for shot peening and performing catch tests on it?
Thanks!
I'm trying to perform catch tests for flow valve calibration on an equipment that uses MIL-11 (AGB-10) glass bead. This grade being very fine, I'm having problems finding a way to keep the media in the catch test container without causing restriction for the air to get out. Anyone has experience in using this media for shot peening and performing catch tests on it?
Thanks!