Peening of Bisaloy Weld - 03/04/05 11:05 AM
Dear Sir/Madam,
A customer of mine wishes to Shot Peen a Substrate of Bisaloy for the purpose of Relieving Stress and Strengthening the Weld around a Large Ship Rudder. The client has no reference as to the Peening Intensity required. Is their a formula for this? Also can you Peen for too long a period and in fact weaken the join?
Regards
Mark
A customer of mine wishes to Shot Peen a Substrate of Bisaloy for the purpose of Relieving Stress and Strengthening the Weld around a Large Ship Rudder. The client has no reference as to the Peening Intensity required. Is their a formula for this? Also can you Peen for too long a period and in fact weaken the join?
Regards
Mark