Masking part - 08/04/99 07:07 PM
Hello,
I need to protect the marking of a small part from shot-peening. The area to be protected is very small and it is important not to mask a larger area for stress concerns.
It is not easy for this application to use a permanent mask. I was wondering if there are some tapes or maybe silicon rubber that could stand shot-peen over 6A intensity. The surface to be protected is 0.090" x 0.090".
Parameters: AMS 2432, AWC 12, 6A
Any idea?
Thanks,
Benoit Gilbert
Pratt & Whitney Canada
I need to protect the marking of a small part from shot-peening. The area to be protected is very small and it is important not to mask a larger area for stress concerns.
It is not easy for this application to use a permanent mask. I was wondering if there are some tapes or maybe silicon rubber that could stand shot-peen over 6A intensity. The surface to be protected is 0.090" x 0.090".
Parameters: AMS 2432, AWC 12, 6A
Any idea?
Thanks,
Benoit Gilbert
Pratt & Whitney Canada