Home
Posted By:
Jack Champaigne
Almen intensity verification policy
-
08/16/09
05:26 PM
Assume the intensity has been determined properly (minimum of 4 strips and arc height at T1 increases by 10% at T2). How should Almen intensity verification be performed?
©