AMS 2430 marginal shapes - 01/25/05 03:24 PM
Dear shotpeener,
I have to verify something about AMS 2430 M.
According to the shape maintenance requirement of cast steel shot, the allowance of "Marginal Shape" is removed.
Shall "Marginal shape" be included in "Unacceptable" or "Acceptable" ?
Please let me know the instruction.