AMS 2430 Cast Steel Shot Conditioning - 03/26/04 01:12 PM
Paragraph 3.1.1.1 of AMS 2430 requires conditioning of new cast steel shot to remove scale. My machines have autofill capability which adds media as required. Also, my machines have classifiers so media is added in small amounts when needed. This makes it difficult to condition the media.
The media when received does not have scale and meets all requirements of AMS 2431/1. Do I need to condition it? Can I write my procedures to condition only if scale is identified at receiving? How is everyone else meeting this requirement?
The media when received does not have scale and meets all requirements of AMS 2431/1. Do I need to condition it? Can I write my procedures to condition only if scale is identified at receiving? How is everyone else meeting this requirement?