AS13100 MSA for Almen Gage - 03/10/22 03:57 PM
AS13100 AESQ Quality Management System Requirements for Aero Engine Design and Production Organizations
If you're processing parts for any of the major aero engine manufactures you have less than a year to get your QMS updated
to include these supplemental requirements.
I'm looking for a little help on this:
Anyone come up with a method to comply with AS13100 section 7.1.5.1.1 of AS13100 Measurement Systems Analysis (MSA)? for the Almen Gage? or perhaps even Magnavalves?
Thanks,
Walter Beach
If you're processing parts for any of the major aero engine manufactures you have less than a year to get your QMS updated
to include these supplemental requirements.
I'm looking for a little help on this:
Anyone come up with a method to comply with AS13100 section 7.1.5.1.1 of AS13100 Measurement Systems Analysis (MSA)? for the Almen Gage? or perhaps even Magnavalves?
Thanks,
Walter Beach