AMS-2431/6 Glass Bead - 02/02/07 10:04 PM
Lately we have been rejecting an awful lot of glass bead at incoming inspection. The glass in question is failing at sieve inspection, and it’s not even close.
I’m wondering if anyone else has been experiencing similar problems? The manufacturer has not been very helpful in resolving the issue. It appears to me that they may not be all that interested in the peening market. If so this is a major issue.