go-no-go gage - 06/20/08 05:00 PM
Hi Jack,
I would like clarifiaction regarding go-no-go gages. We are using 3/8" orifice nozzles for our automated shot peen machine. The first question the Nad CAp auditor asked me was how are you making sure your nozzles are in spec. I told him with a go-no-go gage. That was the correct answer but what are the requirements of the gage with respect to a 3/8" nozzle?
Thanks Jack,
Sue
Skills, Inc.
I would like clarifiaction regarding go-no-go gages. We are using 3/8" orifice nozzles for our automated shot peen machine. The first question the Nad CAp auditor asked me was how are you making sure your nozzles are in spec. I told him with a go-no-go gage. That was the correct answer but what are the requirements of the gage with respect to a 3/8" nozzle?
Thanks Jack,
Sue
Skills, Inc.