Posted By: Y.S. Almen strip position - 08/08/21 06:41 AM
What is the best position of almen strip for intensity verification, horizontal or vertical? The case is shaded almen strip, representing small blade slots. I ask because sometimes I see the strip positioned vertically, although in my opinion it should be horizontally.
Thank you in advance.
Posted By: Jack Champaigne Re: Almen strip position - 08/09/21 02:48 PM
You should choose an orientation that best represents your peening setup. Without photos, it isn't easy to give any more advice.