Hello every one,
Hope you are doing good and staying safe.
My question is which parameter i should remain the same as parameters at intensity point to apply on peening actual part:
1. Shot type and size (sure)
2. Impact angle (sure)
3. Stand off distance (sure)
3. Shot Feed rate (not sure)
4. Nozzle size (sure)
5. Translation speed of nozzle.(not sure)
6. Blasting pressure. (not sure)
7. Rotary speed of part.(not sure)
Because i want to change some parameters above to control the required coverage. Thank you for your support.
Last edited by donhan; 10/21/20 04:23 AM.