Can anyone point me in the right direction of any reference data regarding what intensities can be achieve by nozzle sizes at varying air pressures and media size?

Top
#1137 - 02/28/15 12:54 PM Re: Nozzle Performance [Re: tec]
Jack Champaigne Offline


Registered: 04/20/99
Posts: 325
Loc: Mishawaka, IN, USA
Download this guide from our web site:

http://www.shotpeener.com/learning/nozzle.pdf