#1248 - 09/06/16 04:41 AM Shot peening an induction hardened part.
Sinbad Offline
Member

Registered: 09/15/13
Posts: 7
Loc: Sweden
Hello,
I wonder if you can give me some tips regarding shot peen an induction hardened steel part. Is it going to be beneficial to perform the peening after this kind of heat treatment? do you have articles?

Top
#1249 - 09/06/16 01:37 PM Re: Shot peening an induction hardened part. [Re: Sinbad]
Jack Champaigne Offline


Registered: 04/20/99
Posts: 320
Loc: Mishawaka, IN, USA
Go to shotpeener.com and go to the library. Search for the term "induction hardened". I saw 132 links when I did this search.
Good luck.
jack

Top
#1250 - 09/07/16 03:03 AM Re: Shot peening an induction hardened part. [Re: Sinbad]
Sinbad Offline
Member

Registered: 09/15/13
Posts: 7
Loc: Sweden
I did that before writing here but couldn't find a clear relation between shot peening and induction hardening.

Top
#1251 - 09/07/16 09:41 AM Re: Shot peening an induction hardened part. [Re: Sinbad]
Charlie Offline
Member

Registered: 09/23/14
Posts: 16
Loc: USA
http://www.shotpeener.com/library/detail.php?anc=1984035&keyword=induction+hardening

Sinbad,
This article may give your answer, if it doesn't then let us know and we will try to help again.

Top
#1262 - 09/09/16 10:11 AM Re: Shot peening an induction hardened part. [Re: Sinbad]
Sinbad Offline
Member

Registered: 09/15/13
Posts: 7
Loc: Sweden
Yes, I read this article.
The thing is that the data provides only shallow information about residual stresses. Although the results from the fatigue test looks good but questions like how the residual stresses look both at the surface and in depth as a profile, are very interesting.
These kind of information that I'm looking really for.