Many types of furniture like chair, table, cupboard etc are manufactured nowadays. But after manufacturing there will be a lot of irregularities in the furniture which makes the furniture difficult to be painted. In order to clean away this irregularities can we use shot peening technique. Will this technique make the furniture ready for painting?
People can make use of online essay services in order to obtain professional custom essay.

Top
#1391 - 09/06/18 04:04 PM Re: Using shot peening in metallic furnitures? [Re: JuneDScott]
Charlie Offline
Member

Registered: 09/23/14
Posts: 16
Loc: USA
Yes, though not generally referred to as shotpeening. Abrasive blasting or abrasive cleaning is a widely used method of surface preparation for metallic parts that are to receive organic finishes.