Donhan
I would suggest going back to your customer and asking them to define the shot requirement. Maybe they could inform you of the media specification. 550 size is normally associated with cast steel shot which is magnetic. There is stainless cut wire, glass and ceramic peening media.
Edited by Dennis Scharer (01/30/18 07:44 AM)