The answer is "It depends". If the parameters were submitted to the customer then changes to the parameters would need to be re-submitted. Running another job in the same machine would constitute a change in parameters even if the parameters were returned to the original settings. Something may have changed. The safe thing to do is run a new saturation curve unless the customer agrees that going back to previous parameter settings is acceptable. (Make sure to get it in writing....).