Hi all;
As we know intensity is independent of time,but coverage not.
Recently,i'm reading a process sepc(ABP1-2028) in which it is written as "The peening time, or part feed rate, shall be selected such that the required intensity in each location is achieved and the coverage requirements of are met."
It looks like peening time affect intensity? what do you think about the sentence?