It was decided that title of the specifications will add the word spherical and spherically where applicable through out the documents.
Example: AMS 2431/3
Was: Conditioned Carbon Steel Cut Wire Shot, Regular Hardness
(45 to 52 HRC)
Now: Spherically Conditioned Carbon Steel Cut Wire Shot, Regular Hardness (45 to 52HRC)